People make repairs in apartments all the time, this process is continuous, because over time everything wears out, deteriorates or breaks. When it comes to the bathroom, the question arises as to what to do with a cast iron bathtub. Many believe that now they cannot find products of the same quality as they were produced before, and therefore do not want to get rid of the old one. Others would like to replace it with a new one, but don't want to chip the tiles, damage the floor tiles, or scratch the doors that can occur when replacing. In such cases, a bulk bath will be the solution. Reviews about her speak volumes. Almost everyone who ordered such a procedure was satisfied with the result.
Now several types of material are used to make the new bulk bath shine with bright colors. Liquid acrylic is the most widely used. Its use eliminates the need for a brush, which is required when applying enamel and can leave traces of scratches. Liquid acrylic is simply poured into a cleaned and degreased bath. This option is better than installing an acrylic liner, because it needs to be sized, bent over the edges, and for this you will have to remove the adjacent tile. In addition, there may be space between the tub and the liner. Bacteria and mold will grow there. A bulk acrylic bath will save the user from such thoughts, because there will be no gaps between the main part and the coating. Full contact of the layers which are not passing air and moisture is guaranteed. For consumers, the hygienic conditions provided by the bulk bath are important. Reviews about her confirm this fact.
Process Features
If you decide to install such a self-leveling coating at home, carefully study the information about the company providing these services before calling the wizard. It must have the necessary certificates for the materials used, give written guarantees for the repair of poor-quality coatings. Well, if one of your friends has already used the services of the chosen organization, then there is confidence that this is not a one-day firm that carries out such work. Some people fell for the offers of unscrupulous performers. As a result, the white surface of the hot tub turned yellow, bubbled, cracked and chipped, and owners had to look for other well-reputed tub fillers. Usually, defects appear due to the fault of an employee who incorrectly performs the process. The work cannot take an hour and a half, because a thorough cleaning of the bathtub is required first. The filling itself takes less than an hour. The total working time is about three hours, after which you will have to wait 4 days and not use the bathroom during this time. Of course today thereand faster-drying materials, such as stacryl dries in 36 hours. But even in this case, you can not use the product for its intended purpose during the specified period. The result of a properly carried out processing process will be a sparkling bulk bath. User reviews testify to this.
It is better to entrust such work to professionals, but if you wish, you can handle everything with your own hands. If you decide that your goal is a bulk bath, the reviews of those who have already done such work on their own will help to cope with the task. A modern coating will last 5-10 years, will delight with strength, warmth, whiteness and ease of use.